How to Eliminate Internal Stress in Injection Molded Products?
Causes of Internal Stress in Injection Molded Products
Internal stress refers to the residual stress generated during the injection molding process due to uneven material shrinkage, differences in cooling rates, or molecular chain orientation. The main causes include:
- Uneven cooling: Thick-walled areas cool more slowly than thin-walled sections, leading to shrinkage differences.
- Insufficient packing: Inadequate melt compensation results in internal voids or shrinkage stress.
- Molecular orientation: During high-speed filling, polymer chains align along the flow direction, and after cooling, anisotropic stress is formed.
Core Methods to Eliminate Internal Stress
Process Optimization
- Adjust melt temperature: Properly increasing melt temperature (e.g., PC: 260–300℃) reduces viscosity and lowers orientation stress. However, excessive temperature may cause degradation.
- Control packing pressure and time: Packing pressure is typically 50–80% of injection pressure. Packing time should cover gate solidification (usually 5–15 seconds).
- Reduce injection speed: High-speed injection increases molecular orientation. It is recommended to use multi-stage speed control, with lower speed in the final filling stage.
Material Selection
- Choose materials with low shrinkage: For example, ABS has a shrinkage rate of 0.4–0.7%, which is better than PS (0.6–0.8%).
- Add toughening agents: Adding POE can reduce internal stress, but the dosage should be controlled (generally 5–10%).
Post-Treatment Techniques
- Annealing: Heat the product below the glass transition temperature (e.g., PP: 80–100℃ for 1–2 hours) to relax molecular chains.
- Moisture conditioning: Nylon products can be treated by boiling water bath (100℃ for 2 hours) to balance crystallinity.
Design Improvements
- Uniform wall thickness: Avoid sudden wall thickness changes, and keep variation within 20%.
- Optimize gate position: Prefer fan-shaped or submarine gates with balanced flow to reduce weld lines.
Precautions
- Avoid excessive annealing: If temperature exceeds the heat distortion temperature (e.g., PC: 130–140℃), product deformation may occur.
- Mold temperature control: Higher mold temperatures (e.g., 80–120℃) can reduce cooling stress but may increase cycle time. Parameters should be adjusted based on material characteristics.
By comprehensively applying the above methods, internal stress can be significantly reduced, improving dimensional stability and mechanical strength. In actual production, it is essential to fine-tune parameters according to the specific material and product design.
Factory Overview
Latest Post
The Importance of Injection Mold Temperature Control and Common Methods
How to Optimize the Cooling System of Injection Mold?
How Electronic Injection Molds Meet the Needs of Complex Structures?
Analysis of the Process of Injection Molding of Electronic Products
The Importance of Electronic Injection Mold in the Modern Manufacturing Industry
Influence of Injection Molding of Electronic Products on Material Selection
Call
+86-0769-86066062
info@kehuimold.com
Service Time
9:00 AM – 10:00 PM